Replacing glazing with polishing is still controversial in terms of the surface roughness of dental porcelains. This study investigated the polishing performance of a ceramic-polishing rubber wheel (CP-RW), which contains large uniform and rounded silicon carbide particles and small diamond particles, in improving the surface roughness of two feldspathic porcelains for sintering and CAD/CAM milling. Using a confocal laser scanning microscopy, the changes in the surface roughness parameters were evaluated before and after polishing or glazing for three surface treatment groups: SofLex polishing, CP-RW polishing, and Glazing. Regardless of the parameters, all treatments reduced roughness values (repeated measures ANOVA, p<0.05). The roughness values obtained after CP-RW polishing were lower than those obtained after SofLex polishing and glazing (2-way ANOVA, p<0.05). Polishing both ceramics with CP-RW made the surfaces smooth with the lowest roughness values in all parameters. The effect was dependent on the materials used.
No clinical trial protocols linked to this paper
Clinical trials are automatically linked when NCT numbers are found in the paper's title or abstract.PICO Elements
No PICO elements extracted yet. Click "Extract PICO" to analyze this paper.
Paper Details
MeSH Terms
Associated Data
No associated datasets or code repositories found for this paper.
Related Papers
Related paper suggestions will be available in future updates.