Fracture strengths of endocrown restorations fabricated with different preparation depths and CAD/CAM materials.

, , , , ,

Dental materials journal Vol. 37 (2) : 256-265 • Mar 2018

The objectives of this study were to compare the fracture strength of endocrown restorations fabricated with different preparation depth and various CAD/CAM ceramics, and to assess the fracture types. Endodontically treated 100 extracted human permanent maxillary centrals were divided into two preparation depth groups as short (S: 3-mm-deep) and long (L: 6-mm-deep), then five ceramic subgroups, namely: feldspathic-ceramic (Vita Mark II-VM2), lithium-disilicate glass-ceramic (IPS e.max CAD-E.max), resin-ceramic (LAVA Ultimate-LU), polymer infiltrated ceramic (Vita Enamic-VE) and monoblock zirconia (inCoris TZI-TZI) (n=10/subgroup). The endocrowns were fabricated by CAD/CAM and were cemented with resin cement (RelyX U200). The teeth were thermally cycled (5,000cycles) and fracture tests were performed at 45 masculine angle to the teeth. The data were statistically analyzed (Kruskal-Wallis, Mann Whitney U), failure modes were evaluated with stereomicroscopy. Zirconia group provided the statistically highest fracture strength, but also exhibited non-repairable failures. Preparation depth has an effect on the fracture strength only for feldspathic ceramic.

No clinical trial protocols linked to this paper

Clinical trials are automatically linked when NCT numbers are found in the paper's title or abstract.
PICO Elements

No PICO elements extracted yet. Click "Extract PICO" to analyze this paper.

Paper Details
MeSH Terms
+1 more
Associated Data

No associated datasets or code repositories found for this paper.

Related Papers

Related paper suggestions will be available in future updates.