Adhesive Failure of Lava Ultimate and Lithium Disilicate Crowns Bonded to Zirconia Abutments: A Prospective Within-Patient Comparison.

, , ,

The International journal of prosthodontics Vol. 31 (3) : 208-210 • May 2018

PURPOSE: To demonstrate the influence of restorative material on the success of clinical bonding to zirconia. MATERIALS AND METHODS: A total of 50 participants with a single implant received screw-retained restorations; ie, Lava Ultimate (LU) crowns extraorally bonded to zirconia abutments. After 1 year, lithium disilicate (LDS) was used as an alternative restorative material. These restorations were also followed for 1 year. RESULTS: Forty LU restorations (80%) debonded within 1 year of clinical service, whereas no bonding failures occurred with LDS restorations. CONCLUSION: The choice of restorative material for single crowns luted to zirconia implant abutments strongly influences the incidence of bonding failures.

No clinical trial protocols linked to this paper

Clinical trials are automatically linked when NCT numbers are found in the paper's title or abstract.
PICO Elements

No PICO elements extracted yet. Click "Extract PICO" to analyze this paper.

Paper Details
MeSH Terms
Associated Data

No associated datasets or code repositories found for this paper.

Related Papers

Related paper suggestions will be available in future updates.