PURPOSE: The objective of this in vitro study was to evaluate the shear bond strength (SBS) of several universal adhesives to dentin treated with sodium hypochlorite (NaOCl), and NaOCl followed by ethylenediaminetetraacetic acid (EDTA). MATERIALS AND METHODS: Adhese Universal, Scotchbond Universal, Prime & Bond Elect, Prime & Bond Active, and Optibond XTR were included in the study. SBS values were determined in self-etch mode with no pretreatment of the dentin, after a 20-minute exposure of the dentin to 6% NaOCl, and after a 20-minute exposure to NaOCl followed by a one-minute exposure to 17% EDTA. Experimental groups were repeated using a total-etch technique (except Optibond XTR). RESULTS: Adhesives in self-etch mode had significantly reduced SBS following dentin exposure to NaOCl (P < .05), while with a total-etch technique, only Prime & Bond Active was affected (P < .05). SBS in self-etch mode when NaOCl exposure was followed by EDTA were equal to or higher than negative control values (P < .05). For total-etch groups, Adhese Universal was negatively affected by NaOCl + EDTA exposure (P < .05). Prime & Bond Elect exhibited lower SBS following NaOCl + EDTA exposure when compared to just NaOCl exposure but was not different from the negative control (P < .05). CONCLUSION: For the adhesives tested, the use of 17% EDTA following NaOCl exposure negated the negative effects of NaOCl on SBS in self-etch mode. When used in total-etch mode, results varied significantly, with some adhesives performing better or worse depending on the specific testing condition.
No clinical trial protocols linked to this paper
Clinical trials are automatically linked when NCT numbers are found in the paper's title or abstract.PICO Elements
No PICO elements extracted yet. Click "Extract PICO" to analyze this paper.
Paper Details
MeSH Terms
Associated Data
No associated datasets or code repositories found for this paper.
Related Papers
Related paper suggestions will be available in future updates.